Molecular sieve production method

There are hydrothermal synthesis, hydrothermal conversion and ion exchange methods:

1. The hydrothermal synthesis method is used to prepare products with higher purity and to synthesize molecular sieves that do not exist in nature. Mix the silicon-containing compound (water glass, silica sol, etc.), aluminum-containing compound (hydrated alumina, aluminum salt, etc.), alkali (sodium hydroxide, potassium hydroxide, etc.) and water in an appropriate ratio, and heat in the autoclave After a certain period of time, molecular sieve crystals are precipitated. The synthesis process can be expressed by the following formula:


In the industrial production process, Na-molecular sieve is generally synthesized first, such as the synthesis of 13X and 10X molecular sieves (see figure). Adding certain additives in the hydrothermal synthesis process can change the structure of the final product. For example, adding a quaternary ammonium salt can obtain a ZSM-5 molecular sieve.


2. Hydrothermal conversion method "In the presence of excess alkali, the solid aluminosilicate is hydrothermally converted into a subsieve. The raw materials used are kaolin, bentonite, diatomite, etc., and synthetic silica alumina gel particles can also be used. This method has low cost, but the product purity is not as good as hydrothermal synthesis.


3. Ion exchange method "Usually the Na-molecular sieve is converted into a molecular sieve containing the required cations in an aqueous solution. The general formula is as follows:

In the formula, Z- represents the anion skeleton, Me+ represents the cation to be exchanged, such as NH, Ca2+, Mg2+, Zn2+, etc. The raw materials are usually chloride, sulfate, nitrate. The difficulty of exchanging cations of different properties on the molecular sieve is different, which is called the selection order of the molecular sieve. For example, the selection order of the 13X molecular sieve is Ag+, Cu2+, H+, Ba2+, Au3+, Th4+, Sr2+, Hg2+, Cd2+, Zn2+, Ni2+, Ca2+, Co2+, NH, K+, Au2+, Na+, Mg2+, Li+. The following parameters are commonly used to express the exchange result: exchange degree, that is, the percentage of the amount of Na+ exchanged to the original Na+ amount in the molecular sieve; exchange capacity, which is the number of milligram equivalents of cations exchanged per 100 grams of molecular sieve; exchange efficiency, which means the exchange of cations in the solution to The mass percentage on the molecular sieve. In order to prepare a suitable molecular sieve catalyst, it is necessary to mix the exchanged product with other components. These components may be other catalytically active components, co-catalysts, diluents or binders, etc. The prepared materials can be shaped. Perform catalyst activation.